首页> 外国专利> Process for producing cast pieces of spheroidal graphite with high geometrical and dimensional precision and improved mechanical properties

Process for producing cast pieces of spheroidal graphite with high geometrical and dimensional precision and improved mechanical properties

机译:具有高几何和尺寸精度以及改善的机械性能的球形石墨铸件的生产方法

摘要

The manufacturing process uses cast iron containing the following materials (percentage weight in brackets): C (3 - 4); Si (1.7 - 3); Mn (0.1 - 0.7); Ni (0 - 4); Cu (0 - 1.5); Mo (0 - 0.5); residual Mg (0.025 - 0.080), and the remainder iron and impurities, poured in a liquid state at a temperature of 1350 - 1550 degrees C. The cast iron is essentially bainitic, perlitic or ferritic in structure, and moulded blanks made from it have a volume more or less identical to the finished component and are shaped by hot plastic deformation using calibration in containers or closed matrices to avoid any side burrs.
机译:制造过程使用的铸铁包含以下材料(括号中的重量百分比):C(3-4); Si(1.7-3);锰(0.1-0.7);镍(0-4);铜(0-1.5); Mo(0-0.5);残留的Mg(0.025-0.080)以及其余的铁和杂质在1350-1550摄氏度的温度下呈液态浇铸。铸铁的结构基本上是贝氏体,珍珠岩或铁素体,并且由其制成的模制坯料具有体积与成品零件大致相同,并通过在容器或密闭基质中进行校准而通过热塑性变形成型,以避免产生任何侧边毛刺。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号