首页> 外国专利> River for pitting corrosion resistance and excellent chemical tank of sulfuric acid is corrosive seawater from

River for pitting corrosion resistance and excellent chemical tank of sulfuric acid is corrosive seawater from

机译:耐点蚀的河流和优良的硫酸化工罐是腐蚀性海水

摘要

for a chemical tank which can suppress the formula due to corrosion damage due to sulfuric acid and brine to provide a river , by mass %, C: 0.003~0.05%, Si: 5% or less , Mn: not more than 2%, P: less than 0.03%, S: 0.010% or less , 0: 0.0050% or less , Cr: 18~25%, Ni : 10~20%, Mo: 1.0~4.5%, Cu: 1.0~3.0%, N: include from 0.05 to 0.3% , and a remainder of the steel of Fe and inevitable impurities , the display -containing components in mass% and a GI = [Cr] + 1.6 [Ni] + 6.0 [Mo] + 7.1 the value of [Cu] , more than 75 , 88 or less, and , PI = indicating the contained components , in mass % [Cr] + 1.3 [Mo] + 1.4 [Cu] + 2.2 [N] of the value of more than 23 , for excellent chemical tank corrosion and pitting corrosion of sulfuric acid is less than 32 , characterized in that river .
机译:对于可以抑制由硫酸和盐水引起的腐蚀破坏引起的化学式产生化学侵蚀的化学罐,以质量%计,C:0.003〜0.05%,Si:5%以下,Mn:不大于2%, P:小于0.03%,S:0.010%以下,0:0.0050%以下,Cr:18〜25%,Ni:10〜20%,Mo:1.0〜4.5%,Cu:1.0〜3.0%,N :包括0.05%至0.3%,以及剩余的钢中的Fe和不可避免的杂质,以质量%计的显示器所含成分和GI = [Cr] + 1.6 [Ni] + 6.0 [Mo] + 7.1 [Cu]大于75,小于等于88,并且PI =表示所包含的成分,以质量%[Cr] + 1.3 [Mo] + 1.4 [Cu] + 2.2 [N]表示,大于23,用于优良的化学槽腐蚀和硫酸的点蚀小于32,其特点是河流。

著录项

  • 公开/公告号KR100545750B1

    专利类型

  • 公开/公告日2006-01-24

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20030029001

  • 申请日2003-05-07

  • 分类号C22C38/40;

  • 国家 KR