首页> 外国专利> PRODUCTION METHOD OF METAL IMPREGNATED POLYMER ELECTROLYTE MEMBRANE USING SUPERCRITICAL FLUID AND THE POLYMER ELECTROLYTE MEMBRANE MADE BY THE METHOD

PRODUCTION METHOD OF METAL IMPREGNATED POLYMER ELECTROLYTE MEMBRANE USING SUPERCRITICAL FLUID AND THE POLYMER ELECTROLYTE MEMBRANE MADE BY THE METHOD

机译:超临界流体制备金属浸渍高分子电解质膜的方法及由该方法制得的高分子电解质膜

摘要

A metal-impregnated polymer electrolyte membrane is provided to have remarkably reduced methanol permeability and improved ion conductivity and to produce a fuel cell having excellent voltage and power density characteristics according to current density. The metal-impregnated polymer electrolyte membrane is manufactured by the steps of: impregnating a polymer electrolyte membrane with a metal precursor using supercritical fluid; and reducing the metal precursor impregnated in the polymer electrolyte membrane. The supercritical fluid is at least one selected from carbon dioxide, methane, ethane, ethylene, nitrous oxide, ammonia, and methanol. The metal precursor is an organic ligand compound of a transition metal element.
机译:提供一种浸渍有金属的聚合物电解质膜,其具有显着降低的甲醇渗透性和改善的离子电导率,并生产根据电流密度具有优异的电压和功率密度特性的燃料电池。金属浸渍的聚合物电解质膜通过以下步骤制造:使用超临界流体将聚合物电解质膜用金属前体浸渍;和将聚合物电解质膜浸渍在金属电解质中。还原浸渍在高分子电解质膜中的金属前体。超临界流体是选自二氧化碳,甲烷,乙烷,乙烯,一氧化二氮,氨和甲醇中的至少一种。金属前体是过渡金属元素的有机配体化合物。

著录项

  • 公开/公告号KR100682030B1

    专利类型

  • 公开/公告日2007-02-15

    原文格式PDF

  • 申请/专利权人 FUELCELLPLUS TECH;

    申请/专利号KR20050131132

  • 发明设计人 SAUK JUN HO;BYUN JUNG YEON;SAUK KYOUNG HO;

    申请日2005-12-28

  • 分类号H01M8/10;H01M8/02;

  • 国家 KR

  • 入库时间 2022-08-21 20:32:58

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号