CONCRETE AND MORTAR COMPOSITION FOR IMPROVING IMPACT SOUND RESISTANCE AND METHOD OF IMPROVING IMPACT SOUND RESISTANCE OF CONCRETE SLAB FLOOR-CEILING

机译:改善冲击声阻力的混凝土和砂浆组合物以及改善混凝土楼板的冲击声阻力的方法

摘要

A concrete or mortar composition for noise insulation and a method for improving noise resistance of concrete slab floor-ceiling by using the composition are provided to reduce preparation steps of concrete or mortar for noise insulation so as to reduce preparation cost and time and to improve compressive strength and impulse noise resistance of the prepared concrete or mortar by employing styrene-butadiene synthetic rubber latex combined with surfactant for the concrete or mortar composition. A concrete or mortar composition for noise insulation comprises styrene-butadiene synthetic rubber latex(SBR) that comprises anionic surfactant and nonionic surfactant in the ratio of [1:9]-[9:1] by weight, and the composition is laminated on concrete slab in a thickness of 3-10cm. The anionic surfactant is at least one selected from a group consisting of olefin sulfonate, alkylbenzene sulfonic acid, alkyl ether sulfate, cocoyl isetionate and lauroyl sarcosinate. The nonionic surfactant is at least one selected from a group consisting of glyceryl ester, amine oxide, alkanol amide and sorbitan ester. The composition laminated on the concrete slab forms plural proximal protrusion. The composition for noise insulation optionally comprises fiber selected from polypropylene, polyester, nylon and acrylic fiber. The composition optionally comprises 0.2-1.5 parts by weight of silicone wetting agent or hydrocarbon wetting agent with respect to 100 parts by weight of styrene-butadiene synthetic rubber latex. The composition optionally comprises 1-15 parts by weight of at least one organic binder selected from a group consisting of acrylic acid, acrylic acid copolymer, vinyl acetate, vinyl acetate copolymer, polyvinyl alcohol and vinyl acetate. The composition optionally comprises 3-5 parts by weight of gypsum or waste gypsum.
机译:提供了一种用于隔音的混凝土或砂浆组合物以及通过使用该组合物来改善混凝土板地板天花板的抗噪声性的方法,以减少用于隔音的混凝土或砂浆的制备步骤,从而降低了制备成本和时间并改善了压缩性。通过将苯乙烯-丁二烯合成橡胶胶乳与表面活性剂结合用于混凝土或砂浆组合物,可以使所制备的混凝土或砂浆的强度和抗冲噪声性能。用于隔音的混凝土或砂浆组合物包含苯乙烯-丁二烯合成橡胶胶乳(SBR),该胶乳包含阴离子表面活性剂和非离子表面活性剂,其重量比为[1:9]-[9:1],并将该组合物层压在混凝土上板厚3-10cm。所述阴离子表面活性剂是选自由烯烃磺酸盐,烷基苯磺酸,烷基醚硫酸盐,椰油基羟乙基磺酸盐和月桂酰基肌氨酸盐组成的组中的至少一种。非离子表面活性剂是选自甘油酯,氧化胺,链烷醇酰胺和脱水山梨糖醇酯中的至少一种。层压在混凝土板上的组合物形成多个近端突起。用于隔音的组合物任选地包含选自聚丙烯,聚酯,尼龙和丙烯酸纤维的纤维。相对于100重量份的苯乙烯-丁二烯合成橡胶胶乳,所述组合物任选地包含0.2-1.5重量份的硅酮润湿剂或烃润湿剂。该组合物任选地包含1-15重量份的至少一种选自丙烯酸,丙烯酸共聚物,乙酸乙烯酯,乙酸乙烯酯共聚物,聚乙烯醇和乙酸乙烯酯的有机粘合剂。该组合物任选地包含3-5重量份的石膏或废石膏。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号