METHOD FOR PROCESSING carnallite dust from the cyclone furnace fluidized bed

机译:从旋风炉流化床处理角砾岩粉尘的方法

摘要

1. Method for processing carnallite dust cyclone of a fluidized bed furnace comprising feeding raw materials into the furnace of the fluidized bed, its dehydration, dust collection in a cyclone followed by removing it from the cyclone, characterized in that the carnallite after dust removal from the cyclones is melted in a container, then the molten carnallite dust molten magnesium chloride is added in a ratio of quantities of molten carnallite dust to the amount of molten magnesium chloride to be (4-6): 1, the mixture is heated to a temperature of 720-850 ° C, lagging ayut and sent for further use as raw material for the electrolytic production of magnesium and hlora.2. A method according to claim 1, characterized in that the dust carnallite melted at 500-580 ° C.3. A method according to claim 1, characterized in that the mixture is settled for 0.5-2.0 p.4. A method according to claim 1, characterized in that as the molten magnesium chloride is used byproduct production titana.5 sponge. A method according to claim 1, characterized in that the dust carnallite SKN.6 melted in the furnace. A method according to claim 1, characterized in that the molten carnallite dust is mixed with the molten magnesium chloride in a mixer SKN furnace.
机译:1.一种处理流化床炉中的角砾石粉尘旋风的方法,包括将原料进料到流化床的炉中,将其脱水,在旋风分离器中收集灰尘,然后将其从旋风分离器中除去,其特征在于,从旋风分离器在一个容器中融化,然后以一定比例(4-6)的比例添加熔融的角矾粉尘与氯化镁的熔融比:1温度为720-850℃,滞后的尤特酒,并进一步用作电解生产镁和绿萝的原料。2。 2.根据权利要求1所述的方法,其特征在于,所述粉煤灰岩在500-580℃下熔融。 2.根据权利要求1所述的方法,其特征在于,所述混合物沉降0.5-2.0p.4。 2.根据权利要求1所述的方法,其特征在于,作为熔融氯化镁使用副产物生产钛5海绵。 2.根据权利要求1所述的方法,其特征在于,粉煤灰岩SKN.6在炉中熔化。 2.根据权利要求1所述的方法,其特征在于,将熔融的角矾粉尘与熔融的氯化镁在混合器SKN炉中混合。

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号