首页> 外国专利> A method for determining a spatial coordinate one point on one of a extrusion tool urgent rod, as well as of a quality characteristic of an extrusion die, an extrusion device or of a material for the production of a profile

A method for determining a spatial coordinate one point on one of a extrusion tool urgent rod, as well as of a quality characteristic of an extrusion die, an extrusion device or of a material for the production of a profile

机译:一种确定挤压工具紧急杆之一上的空间坐标以及挤压模,挤压装置或用于生产型材的材料的质量特性的方法

摘要

Disclosed is a method for determining a spatial coordinate one point on one of a extrusion tool (8) urgent strand (14), where first of all of the strand (14) directly to the extruder head, a pushing sample are separated off and then the position coordinate is measured and based on this method for determining a quality characteristic of an extrusion die (8), an extrusion apparatus (2) or of a material (10) for the production of a profile (11).In order to the possibilities of error in the determination of the quality of an extruded strand (14) to be reduced, it is proposed that the spatial coordinate immediately after the separation of the thrust sample in a non-contacting manner on the further out of the extrusion tool (8) urgent strand (14) is measured.Furthermore, it is proposed that for determining a quality characteristic of an extrusion die (8), first of all under use of a standardized material (10) for the production of a profile (11), a normalized extrusion apparatus (2) and of a standard settings of the extrusion apparatus (2) for determining a quality characteristic of an extrusion apparatus (2), first of all under the use of a standard settings of the extrusion apparatus (2), a standardized extrusion die (8) and a standardized material (10) for the production of a profile (11) and for determining a quality characteristic of a material (10) for the production of a profile (11), first of all under the use of a standardized ..
机译:本发明公开了一种用于确定挤压工具(8)之一的紧急绞合线(14)上的一个点的空间坐标的方法,其中首先将所有绞合线(14)直接连接到挤出机头,将推入的样品分离出来,然后测量位置坐标,并根据该方法确定挤压模(8),挤压设备(2)或材料(10)的质量特性,以生产型材(11)。降低确定挤压条材(14)的质量时可能出现的误差的可能性,建议在以非接触方式将推力样品分离之后,立即将空间坐标进一步从挤压工具中取出( 8)测量紧线(14)。此外,为了确定挤压模(8)的质量特性,建议首先使用标准化材料(10)生产型材(11) ,归一化挤出设备(2)和用于确定挤压设备(2)的质量特性的挤压设备(2)的标准设置,首先要使用挤压设备(2)的标准设置,标准化的挤压模具(8)和标准化的用于制造型材(11)并用于确定用于制造型材(11)的材料(10)的质量特性的材料(10),首先是在标准化的使用下。

著录项

  • 公开/公告号DE102006045101A1

    专利类型

  • 公开/公告日2008-04-03

    原文格式PDF

  • 申请/专利权人

    申请/专利号DE20061045101

  • 发明设计人

    申请日2006-09-21

  • 分类号B29C47/92;G01B21/04;G01B11/03;

  • 国家 DE

  • 入库时间 2022-08-21 19:49:45

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号