The present invention achieve the characteristic of the divided dough is mixed method, even if the water adsorption rate is greater than the adjusted moisture content. I do centrifugal tested A mortar mixture obtained by the pre-adjusting the water content A to mix the fine aggregate was adjusted with water and cement such a constant value. If the water adsorption rate βo obtained by centrifugation test is greater than the adjusted moisture content A, the aggregate surface in adjusting the water content A of the aggregate prior to centrifugation test estimates that there is an unfilled portion of the water, the following equation (1 ) I seek the surface adsorbed water rate βOH by. Q is the water absorption of the interior of the bone material. βOH = {(βo + A) / 2-Q} / (1 + Q / 100) ... (1). Obtaining a primary water W1 which can exhibit the characteristics of the split Mixing method by substituting the surface-adsorbed water βOH rate in the following equation (3). W1 = (α / 100) × C + (βOH / 100) × S ... (3) [Selection Figure] Figure 2
机译:即使水分吸附率大于调整后的水分含量,本发明也实现了面团混合法的特征。我进行了离心测试,通过将水含量A预先调整以混合细骨料而获得的砂浆混合物用水和水泥调整至恒定值。如果通过离心测试获得的吸水率βo大于调整后的水分含量A,则在调整离心测试之前的集料的水分含量A时,集料表面会估计存在水的未填充部分,以下公式( 1)求出表面吸附水率βOH。 Q是骨骼材料内部的吸水率。 βOH= {(βo+ A)/ 2-Q} /(1 + Q / 100)...(1)。通过将表面吸附水的βOH率代入下式(3),得到能够表现出分流混合法的特性的一次水W1。 W1 =(α/ 100)×C +(βOH/ 100)×S ...(3)[选择图]图2

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号