Method for reclaiming soil, sediment and sludge dredged from watercourses contaminated by heavy metals and by dangerous and toxic organic compounds

机译:回收从被重金属和危险有毒有机化合物污染的河道疏dr的土壤,沉积物和淤泥的方法

摘要

A method for reclaiming soil, sediment and sludge dredged from watercourses contaminated by heavy metals and by dangerous and toxic organic compounds characterised in that the soil, sediment or sludge with a water content variable from 5% by weight to 60% by weight is subjected to the following steps:- mixing and homogenizing at a temperature not exceeding 140°C for a time not exceeding two hours with cement binders in a quantity variable from 5% to 50% by weight of the soil, sediment or sludge, to obtain a flowable granular powder with an average diameter between 0,1 mm and 4 mm which is compacted mechanically into briquettes or pellets with a maximum volume of 500 cm3,- a first curing step for cement setting and dehydration of the briquettes for a maximum time of nine days to attain a residual moisture content less than 15%,- a second curing step for a maximum time of twentyeight days.
机译:一种回收被重金属和危险和有毒有机化合物污染的河道疏soil的土壤,沉积物和淤泥的方法,其特征是水分含量从5%到5%变化的土壤,沉积物或淤泥。 60%的重量要经历以下步骤:-在不超过140°C的温度下与不超过2小时的时间混合并均质化,水泥粘合剂的用量为土壤,沉积物或淤泥重量的5%至50%(重量),平均直径介于0.1毫米至4毫米之间,可机械压制成团块或小球,最大体积为500 cm 3 ,-第一个固化步骤,用于水泥定型和煤饼的脱水,最长持续9天,以使残留水分含量小于15%,-第二个固化步骤,最长时间为28天。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号