A modifier composition for warm asphalt mixture is provided to reduce fuel consumption while minimizing emission of harmful materials such as carbon dioxide and to lower optimal mixing temperature and optimal pressing temperature by 15~25 ‹C. A modifier composition for warm asphalt mixture is prepared by heating, melting and mixing, based on a polyamide-based polymer compound 100.0 parts by weight, a low density polyethylene resin 10~30 parts by weight, process oil 35~100.0 parts by weight and polyethylene wax 50~150 parts by weight. A method for manufacturing the modifier composition for warm asphalt mixture comprises a step of adding and mixing the modifier composition for warm asphalt mixture 2~8 parts by weight based on the asphalt 100.0 parts by weight.
机译:提供一种用于热沥青混合料的改性剂组合物,以减少燃料消耗,同时最大程度减少有害物质(例如二氧化碳)的排放,并将最佳混合温度和最佳压制温度降低15〜25°C。通过加热,熔融和混合,基于聚酰胺类聚合物化合物100.0重量份,低密度聚乙烯树脂10〜30重量份,加工油35〜100.0重量份和聚乙烯蜡50〜150重量份一种用于热沥青混合料的改性剂组合物的制造方法,包括以下步骤:添加和混合基于沥青100.0重量份为2〜8重量份的热沥青混合料的改性剂组合物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号