ANATASE TYPE TiO2 NANORODS AND ITS PREPARATION METHOD

机译:锐钛型TiO2纳米粉体及其制备方法

摘要

Provided is a process which includes slowly adding dropwise chilled distilled water to titanium tetrachloride to prepare solution of titanium oxychloride; adding basic solution thereto to maintain pH of the titanium oxychloride solution within a range from 3.5 to 4, thereby providing a suspension of titanium oxyhydroxide precipitate; adding basic solution thereto to adjust the suspension of titanium oxyhydroxide precipitate to be weakly basic, and heating and stirring the mixture at 80 to 100° C.; isolating and collecting dihydroxy-oxotitanium from the heated and stirred suspension of titanium oxyhydroxide precipitate, and washing it with weakly basic aqueous solution; and adding distilled water and 20 to 500 folds of hydrogen peroxide on the basis of 1 mole of Ti4+ in titanium oxyhydroxide to the washed titanium oxyhydroxide, and heat-treating the mixture at a temperature of 90 to 100° C. for 1 to 7 days to prepare titania nanorods having the mean length of 100 nm to 300 nm.
机译:提供了一种方法,该方法包括向四氯化钛中缓慢滴加冷却的蒸馏水以制备三氯氧化钛的溶液。向其中加入碱性溶液以使氯氧化钛溶液的pH保持在3.5至4的范围内,从而提供氢氧化钛沉淀物的悬浮液。向其中加入碱性溶液以调节羟基氧化钛沉淀物的悬浮液为弱碱性,并在80至100℃下加热并搅拌混合物;从加热和搅拌的羟基氧化钛沉淀物的悬浮液中分离并收集二羟基氧钛,并用弱碱性水溶液洗涤。在蒸馏后的氢氧化钛中加入蒸馏水和基于氢氧化钛中1摩尔Ti 4 + 的20至500倍的过氧化氢,并在90-200℃的温度下进行热处理。在100℃下干燥1至7天,以制备平均长度为100nm至300nm的二氧化钛纳米棒。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号