An atmospherically catalyzing and oxidizing method of refractory goldconcentrate with high arsenic and highsulfur, comprises ~ adding predefined ore, solid catalyst, acid and water intoreaction container with stirrers to form ore pulp; ~continuously introducing gas oxidizer such as ozone and oxygen, or ozone andair into the pulp at 60-100°C, continuously stirringthe mixture to form oxidized ore pulp, reacting for 6 to 18 hrs, then coolingto room temperature and filtering; ~ In accordancewith traditional extracting and filtering process, mixing the residue from thefiltering step with calcium hydroxide solution toregulate its pH value to 11 ~ 12, adding sodium cyanide, stirring for 24 hrs,and filtering to extract noble metals from filtrate. Themethod improves the extraction rate of noble metals such as gold and silver inthe refractory gold concentrate while reducing theenvironment pollution.
机译:难熔金的大气催化氧化方法高砷高浓缩硫,包括〜向其中添加预定义的矿石,固体催化剂,酸和水带有搅拌器的反应容器形成矿浆。 〜不断引入气体氧化剂,例如臭氧和氧气,或臭氧和空气在60-100°C下进入纸浆,不断搅拌混合物形成氧化矿浆,反应6至18小时,然后冷却室温过滤〜按照采用传统的萃取和过滤工艺,将用氢氧化钙溶液过滤的步骤将其pH值调节至11〜12,加入氰化钠,搅拌24小时,并过滤以从滤液中提取贵金属。的方法提高了金,银等贵金属的提取率难处理的金精矿,同时减少了环境污染。

著录项

  • 公开/公告号CA2722494A1

    专利类型

  • 公开/公告日2009-12-17

    原文格式PDF

  • 申请/专利权人 DONGHUA UNIVERSITY;

    申请/专利号CA20082722494

  • 发明设计人 LI DENGXING;

    申请日2008-11-25

  • 分类号C22B3/06;C22B3/08;C22B3/10;C22B11/08;

  • 国家 CA

  • 入库时间 2022-08-21 18:42:29

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号