FIELD: chemistry.;SUBSTANCE: thallium metal, containing other elements, is dissolved in sulphuric acid with concentration of 90 to 100 g/l. The solution is evaporated, cooled and the residue is filtered. The obtained solution, which contains thallium sulphate, is filtered and evaporated. Hydrogen sulphide gas is passed through the solution and sulphides of heavy metals are precipitated. Thallium metal is separated by electrolysis. The obtained metal is dissolved in nitric acid and diluted with water to thallium concentration of 60 to 80 g/l. Potassium hydroxide is added until pH equals 10. Using electrolysis, thallium (III) oxide is deposited on the anode and thallium metal is deposited on the cathode. Current density at the anode ranges from 0.25 to 1.00 A/cm2, and from 0.05 to 3.00 A/cm2 at the cathode.;EFFECT: obtaining thallium oxide and thallium metal with low content of impurities maximum 0,0048%, high output of the desired product of minimum 84,2-99,6%, reduced formation of filtrates and pollution of the environment.;2 cl, 1 dwg, 10 ex
机译:领域:化学物质; ::将含其他元素的metal金属溶解于浓度为90至100 g / l的硫酸中。蒸发溶液,冷却并将残余物过滤。将所获得的包含硫酸th的溶液过滤并蒸发。硫化氢气体通过溶液,重金属硫化物沉淀出来。通过电解分离metal金属。将获得的金属溶于硝酸中,并用水稀释至th浓度为60至80 g / l。加入氢氧化钾直至pH等于10。使用电解,将氧化al(III)沉积在阳极上,将metal金属沉积在阴极上。阳极电流密度为0.25至1.00 A / cm 2 ,阴极电流密度为0.05至3.00 A / cm 2 。效果:获得氧化oxide和th杂质含量低的金属最大为0,0048%,所需产物的高产量最小为84,2-99.6%,减少了滤液的形成和对环境的污染。; 2 cl,1 dwg,10 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号