摘要

PPROBLEM TO BE SOLVED: To provide a method of preparing low shrinkage AE concrete using a one component multifunctional admixture satisfying following conditions (1)-(6) at the same time, that are (1) the multifunctional admixture used as one component has excellent stability, which is a prerequisite condition; (2) excellent construction property is secured by suppressing the deterioration with time of flowability and air quantity of the prepared low shrinkage AE concrete for civil engineering; (3) dry shrinkage of a resultant hardened body is low; (4) the resultant hardened body has resistance to freeze-thaw action; (5) the resultant hardened body is slow in the neutralizing speed; (6): the resultant hardened body has reasonable excellent compression strength, and to provide the low shrinkage AE concrete for civil engineering. PSOLUTION: The low shrinkage AE concrete for civil engineering is prepared using cement, water, fine aggregate, coarse aggregate, the multifunctional admixture and an air volume controlling agent, wherein the unit quantity of cement is 280-450 kg/mSP3/SP, the one component multifunctional admixture comprising a specific cement dispersant, a specific dry shrinkage reducing agent and a specific separation reducing agent in a fixed ratio respectively is used by 0.3-3.0 pts.mass per 100 pts.mass cement, and the entrained air is prepared to be 3-8 vol.%. PCOPYRIGHT: (C)2010,JPO&INPIT
机译:

要解决的问题:提供一种使用同时满足以下条件(1)-(6)的单组分多功能掺合料制备低收缩AE混凝土的方法,即(1)多功能掺合料作为一种组件具有出色的稳定性,这是前提条件; (2)通过抑制所制备的用于民用工程的低收缩率AE混凝土随流动性和空气量随时间的恶化而确保优异的建筑性能; (3)所得硬化体的干收缩率低; (4)所得的硬化体具有抗冻融作用; (5)所得硬化体的中和速度慢; (6):所得硬化体具有合理的优异抗压强度,并为土木工程提供低收缩率的AE混凝土。

解决方案:用于民用工程的低收缩AE混凝土是使用水泥,水,细骨料,粗骨料,多功能掺合料和风量控制剂制备的,其中水泥的单位量为280-450 kg / m < SP> 3 是一种以固定比例分别包含特定水泥分散剂,特定干缩减少剂和特定分离减少剂的单组分多功能混合物,用量为每100 pts质量0.3-3.0 pts.mass水泥,夹带的空气准备为3-8 vol。%。

版权:(C)2010,日本特许厅&INPIT

著录项

  • 公开/公告号JP4707197B2

    专利类型

  • 公开/公告日2011-06-22

    原文格式PDF

  • 申请/专利权人 竹本油脂株式会社;

    申请/专利号JP20080273029

  • 申请日2008-10-23

  • 分类号C04B28/02;C04B24/26;C04B24/02;C04B24;C04B103/40;C04B103/44;C04B103/60;C04B111/20;

  • 国家 JP