摘要

PURPOSE: A polyhydroxy resin, a method for manufacturing the same, and an epoxy resin composition using the same are provided to ensure excellent wet-proof property, heat resistance, and fire retardancy as well as excellent moldability and to enable the application to the lamination, molding, and adhesion.;CONSTITUTION: A polyhydroxy resin is represented by chemical formula 1(wherein A represents a naphthalene ring(N) or a benzene ring(B)), wherein a molar ratio calculated by N/(N+B) is 0.2~0.7, a softening point is 75~125°C, and a melting point at 150°C is 2~10Pa·s. A method for preparing an epoxy resin comprises a step of racing the polyhydroxy resin with epichlorohydrin.;COPYRIGHT KIPO 2012
机译:用途:提供一种多羟基树脂,其制造方法和使用其的环氧树脂组合物,以确保优异的防湿性,耐热性和阻燃性以及优异的成型性,并使其能够应用于层压组成:多羟基树脂由化学式1表示(其中A表示萘环(N)或苯环(B)),其中摩尔比由N /(N + B)计算熔点为0.2〜0.7,软化点为75〜125℃,熔点为150℃为2〜10Pa·s。环氧树脂的制备方法包括用环氧氯丙烷将多羟基树脂赛车化的步骤。; COPYRIGHT KIPO 2012

著录项

  • 公开/公告号KR20110109939A

    专利类型

  • 公开/公告日2011-10-06

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL CHEMICAL CO. LTD.;

    申请/专利号KR20110027550

  • 发明设计人 NAKAHARA KAZUHIKO;KAJI MASASHI;

    申请日2011-03-28

  • 分类号C08G59/04;C08L63/00;C07C39/14;C07C33/26;

  • 国家 KR

  • 入库时间 2022-08-21 17:50:57

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号