FIELD: metallurgy.;SUBSTANCE: procedure consists in settling plate from electrolyte containing, g/l: nickel chloride 200-350, cobalt chloride 3-11, aluminium oxide 15-40, boric acid 25-40, chloramines B 1.5-4.0, at pH of electrolyte 1.5-5.0, temperature 18-40 °C, cathode current density 0.5-9.0 A/dm2 and in electrolyte mixing. Plate contains, wt %: cobalt 1.8-6.7, aluminium oxide 1.2-3.8, nickel - the rest.;EFFECT: raised wear resistance, adhesion and glide of plate.;2 cl, 2 tbl, 5 ex
机译:领域:冶金学;目的:该程序包括用以下电解液沉降板:g / l:氯化镍200-350,氯化钴3-11,氧化铝15-40,硼酸25-40,氯胺B 1.5-4.0,在电解液pH值为1.5-5.0,温度为18-40°C,阴极电流密度为0.5-9.0 A / dm 2 的条件下以及在电解液混合中。钢板含有重量百分比:钴1.8-6.7,氧化铝1.2-3.8,镍-其余;效果:提高了钢板的耐磨性,附着力和滑动度; 2 cl,2 tbl,5 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号