2. The application relates to a cell structure thermal insulation material, which accounts for 4-96% by weight of a hydraulic polymer labeled before water contact, because it contains at least one stage selected from C3a, CA, C12A7, c11a7caf2, C4A3 '(Yee lemite),C2A (1-x) FX (x genus [0, 1]),The proportion of hydraulic non binder is between 0.3% and 15. Therefore, during these stages, the weight percentage of aquifer accumulated in Al2O3 varies from 4% to 96%, the weight percentage of each load ranges from 4% to 96%, and its volume is porous, ranging from 70% to 70%. ninety-five percent Item 5: foam that can be used to make materials according to any one of items 1 to 4, including: a hydraulic polymer with characteristics before contacting water, because it contains at least one stage selected from C3a, CA, C12A7, c11a7caf2,C4A3 'yée lemite),C2A (1-x) FX (x genus [0, 1]),The non hydraulic phase with Mo C / a ratio between 0.3% and 15, therefore, the proportion of nitrous oxide 3 in the total amount of hydraulic polymer in the two stages is between 3% and 70% by weight, 1% to 30% by weight, and the proportion in the total weight of dry matter in foam is between 3% and 70%, Select at least one load from the reaction load, i.e. at least one aqueous solution and / or non-aqueous solution, and one gas, such as air, carbon dioxide or nitrogen. Item 9: grout that can be used to make materials, according to any item 1 to 4, including: at least,A hydraulic polymer before water contact because it contains at least one stage selected from C3a, CA, C12A7, c11a7caf2, c4a3'yee lemite,C2A (1-x) FX (x genus [0, 1]),The molar C / a ratio of the hydraulic non liquid phase is between 0.3 and 15, so the triggers accumulated in Al2O3 of these stages 3 account for 3% to 70% of the total hydraulic polymer by weight, with at least one low density hollow load, i.e. at least one aqueous solution and / or non-aqueous solution.
机译:2.本申请涉及一种泡孔结构绝热材料,其占水接触之前标记的水硬性聚合物的4-96重量%,因为它包含选自C3a,CA,C12A7,c11a7caf2,C4A3'中的至少一个阶段。 (Yee lemite),C2A(1-x)FX(x属[0,1]),水硬性非粘结剂的比例在0.3%和15之间。因此,在这些阶段中,Al2O3中积累的含水层的重量百分比会发生变化含量为4%至96%,每个负载的重量百分比为4%至96%,其体积为多孔,范围为70%至70%。百分之九十五的项目5:可用于制造项目1-4中任何一项的材料的泡沫,包括:具有水接触特性的水硬性聚合物,因为它包含至少一个选自C3a,CA,C12A7的阶段,c11a7caf2,C4A3'yéelemite),C2A(1-x)FX(x属[0,1]),非水相与Mo C /的比例在0.3%和15之间,因此,一氧化二氮的比例3在两个阶段中,水硬性聚合物总量的比例为3%至70%(重量),1%至30%(重量),泡沫中干物质总重量的比例为3%至70%,选择反应负载中的至少一种负载,即至少一种水溶液和/或非水溶液,以及一种气体,例如空气,二氧化碳或氮气。第9项:根据第1-4项中的任何一项,可用于制造材料的浆液,至少包括:与水接触之前的水硬性聚合物,因为它包含至少一个选自C3a,CA,C12A7,c11a7caf2,c4a3'的级蓝晶石,C2A(1-x)FX(x属[0,1]),摩尔C /水硬性非液相的比率在0.3和15之间,因此这些阶段3的Al2O3中累积的触发因素占占总水硬性聚合物重量的3%至70%,并具有至少一种低密度空心载荷,即至少一种水溶液和/或非水溶液。

著录项

  • 公开/公告号AR079900A1

    专利类型

  • 公开/公告日2012-02-29

    原文格式PDF

  • 申请/专利权人 KERNEOS;

    申请/专利号AR2011P100119

  • 发明设计人 PRAT EVELYNE;FROUIN LAURENT;TAQUET PASCAL;

    申请日2011-01-14

  • 分类号C04B28/02;C04B28/06;

  • 国家 AR

  • 入库时间 2022-08-21 17:25:37

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号