A PROCESS FOR MANUFACTURING BITUMEN / ASPHALT MODIFIER, USING CRUMB RUBBER AND OLEO AMINES

机译:使用碎屑橡胶和油性胺制造沥青/沥青改性剂的过程

摘要

Bitumen/asphalt modifier is manufactured in wet conditions, using expensive polymers either recycled or as fresh ingredients. Cost of manufacture is high and processing time longer. The present invention not only does away with use of any polymeric compounds but relies on dry conditions for manufacture. Oleo amine is added in a small fraction of 5% by weight of batch size. The invention scores in terms of low processing costs and short batch time.
机译:沥青/沥青改性剂是在潮湿条件下制造的,使用的是昂贵的可回收或新鲜成分的聚合物。制造成本高且处理时间更长。本发明不仅取消了使用任何聚合化合物,而且依赖于干燥条件进行制造。以批量大小的5重量%的小部分添加油胺。本发明在低处理成本和短批处理时间方面得分。

著录项

  • 公开/公告号IN252623B

    专利类型

  • 公开/公告日2012-06-01

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN2072/MUM/2008

  • 发明设计人 PARUL RAJENDRA SHAH;

    申请日2008-09-26

  • 分类号C08L95/00;

  • 国家 IN

  • 入库时间 2022-08-21 17:23:58