A process for producing a textured yarn fine false twist polyester yarn comprising subjecting thin polyester multifilament having a single filament fineness of 0.9 dtex or less of a total number of individual filaments 100 to 400 and birefringence of 0.03 to 0.06 at false twist texturing, the method comprising: (1) subjecting the interlacing multifilament yarn to air in order to provide a degree of interlacing of 50 to 90 points interlaced / m measured for yarn false twist texturing, (2) regulate the residence time in a heated draw-false twist to 0.052 to 0.300 seconds and the temperature of filament yarn moving the heater outlet to a temperature higher than the temperature glass transition temperature (Tg) of the polyester polymer at 90 to 140C and subjecting the yarn to multi-filament texturing stretch false twist to a simultaneous a draw ratio of 1.40 to 1.70 times and provide false twist textured yarn, (3) applying a finishing oil in an amount of 1.3 to 3.0% by weight based on the weight of yarn false twist texturing, and (4) winding the resultant yarn under a winding tension of 0.05 to 0.30 cN / dtex at a speed of 500 to 1200 m / min.
机译:本发明的方法,其特征在于,使单丝细度为单根细线100〜400的总数的0.9dtex以下,双折射为0.03〜0.06的细聚酯复丝,该变形丝微细捻聚酯线的制造方法。包括:(1)使交织复丝纱线处于空气中,以提供50/90点的交织度/米,以测量纱线的假捻变形;(2)调节加热牵伸-假捻的停留时间为0.052到0.300秒,长丝纱线的温度将加热器出口移动到高于90到140℃下聚酯聚合物的温度玻璃化转变温度(Tg)的温度,并使纱线同时经受复丝变形拉伸假捻拉伸比为1.40到1.70倍,并提供假捻变形纱,(3)上油量为1.3-3.0%(重量) (4)在0.05至0.30cN / dtex的卷绕张力下以500至1200m / min的速度卷绕所得纱线。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号