首页> 外国专利> A METHOD FOR MANUFACTURING FERRO MOLYBDENUM ALLOY BRIQUETTE FROM THE MIXING POWDER OF MILL SCALE AND MOLYBDENUM OXIDE POWDER BY SOLID-GAS REACTION AND THE BRIQUETTE PRODUCTED BY THE METHOD

A METHOD FOR MANUFACTURING FERRO MOLYBDENUM ALLOY BRIQUETTE FROM THE MIXING POWDER OF MILL SCALE AND MOLYBDENUM OXIDE POWDER BY SOLID-GAS REACTION AND THE BRIQUETTE PRODUCTED BY THE METHOD

机译:一种固相气法从氧化镁粉与氧化铁粉混合粉中制备钼铁压块的方法及所生产的压块

摘要

PURPOSE: Ferro molybdenum alloy briquette and a method of manufacturing ferro molybdenum alloy briquette from the mixed powder of mill scale and molybdenum oxide powder by solid-gas reaction are provided to reduce volatile loss of molybdenum oxide by manufacturing ferro molybdenum alloy power in a power state and lowering the temperature of a process in manufacturing ferro molybdenum alloy by hydrogen reduction. CONSTITUTION: A method of manufacturing ferro molybdenum alloy briquette from the mixed powder of mill scale and molybdenum oxide powder by solid-gas reaction comprises next steps. Mill scale used as a raw material is crushed to a range of 75-150m using ball mill and at the same time, is mixed with oxide molybdenum powder. Hydrogen reduction is made on the mixture at a first low temperature. Hydrogen reduction is continuously made on the mixture at a second high temperature. The ferro molybdenum alloy powder is cooled under hydrogen atmosphere. The ferro molybdenum alloy powder is mixed with wax(Kenolube P11) and is pressed.
机译:用途:提供铁钼合金团块和通过固-气反应由轧制氧化皮和氧化钼粉末的混合粉末制造铁钼合金团块的方法,以通过在功率状态下制造铁钼合金粉末来减少氧化钼的挥发损失通过还原氢来降低制造钼铁合金的过程的温度。组成:一种通过固-气反应由轧制氧化皮和氧化钼粉末制成的混合粉末生产钼铁合金块的方法,包括以下步骤。使用球磨机将用作原料的轧机鳞片粉碎至75-150m的范围,同时将其与氧化物钼粉混合。在第一低温下对混合物进行氢还原。在第二高温下对混合物连续进行氢还原。钼铁合金粉末在氢气氛下冷却。将钼铁合金粉末与蜡(Kenolube P11)混合并压制。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号