PROBLEM TO BE SOLVED: To provide resistance to corrosion and corrosion induced fouling to a metal tube heat exchanger that is subject to a process stream at high temperatures.SOLUTION: A heat transfer component 10 heats the process stream having an inner surface and an exterior surface. The heat transfer component 10 is a tube formed from a steel composition including X, Y, and Z. The tube is the heat transfer component 10 including the following three layers: a base material layer having an arithmetic mean surface roughness of less than 40 micro inches (1.1 m); a Cr-enriched oxide layer formed on at least one of the inner surface and the exterior surface and containing Cr of 10-40 wt.%; and a surface protective layer formed on the surfaces of the Cr-enriched oxide layer including sulfide, oxide, oxysulfide or any mixture thereof.
机译:解决的问题:向经受高温的过程流的金属管热交换器提供抗腐蚀和腐蚀引起的结垢的解决方案:传热组件10加热具有内表面和外表面的过程流。传热部件10是由包含X,Y和Z的钢组合物形成的管。该管是包括以下三层的传热部件10:算术平均表面粗糙度小于40μm的基材层。英寸(1.1 m);在内表面和外表面中至少一个上形成的富Cr氧化物层,其Cr含量为10-40重量%;形成在所述富Cr氧化物层的表面上的表面保护层,所述表面保护层包括硫化物,氧化物,氧硫化物或其任何混合物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号