The present invention provides a method for producing high-purity barium chloride with low strontium and high-purity barium chloride with low strontium. The method comprises following processes: reacting: adding barium carbonate and hydrochloric acid into acid-resistant reactor under agitation to carry out reaction, keeping temperature at 55-60°C, controlling the reaction so as to make pH value of reaction solution at endpoin in a range of 3.5-4.0, after completing reaction, separating solid from liquid to obtain clear filtration containing barium chloride as liquid phase; adjusting process by excess acid: adding the clear filtration containing barium chloride obtained by separation into acid-resistant reactor, adding hydrochloric acid slowly under agitation, controlling [H+] at 2.0-6.0mol/L, cooling the solution until the temperature of the solution is lower than 35°C, then separating solid from liquid, obtaining barium chloride crystal as solid phase; dissolving and removing impurities: dissolving the obtained barium chloride crystal with water to prepare saturated solution at a temperature of 80-90°C, adding hydrogen peroxide, heating the solution to slightly boil, then neutralizing the solution with barium hydroxide to pH 7.0-7.5, separating solid from liquid, obtaining barium chloride-containing solution as liquid phase; and separating and drying: transferring the obtained liquid phase into cooling crystallizer, cooling slowly to 38-42°C, then separating solid from liquid, and drying the obtained solid to obtain the barium chloride product. The purity of high-purity barium chloride with low strontium obtained by the method is equal to 99.60% or more, and Sr content is lower than 10ppm.
机译:本发明提供了一种低锶高纯度氯化钡的生产方法和一种低锶高纯度氯化钡的生产方法。该方法包括以下步骤:反应:在搅拌下向耐酸反应器中加入碳酸钡和盐酸进行反应,将温度保持在55-60℃,控制反应,以使反应液的pH值达到内点。反应完成后,在3.5-4.0的范围内,从液体中分离出固体,得到以氯化钡为液相的澄清过滤。用过量的酸调节工艺:将分离得到的含氯化钡的澄清过滤加入耐酸反应器中,在搅拌下缓慢加入盐酸,将[H +]控制在2.0-6.0mol / L,冷却溶液直至溶液温度低于35℃,然后从液体中分离出固体,得到氯化钡晶体为固相。溶解和除去杂质:在80-90℃的温度下用水溶解所获得的氯化钡晶体以制备饱和溶液,加入过氧化氢,将该溶液加热至略微沸腾,然后用氢氧化钡中和该溶液至pH 7.0-7.5。 ,从液体中分离出固体,得到含氯化钡溶液为液相。分离干燥:将得到的液相转移至冷却结晶器中,缓慢冷却至38-42℃,然后从液体中分离出固体,干燥得到的固体,得到氯化钡产物。通过该方法得到的高纯低锶氯化钡的纯度为99.60%以上,且Sr含量低于10ppm。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号