首页> 外国专利> FABRICATION OF TITANIUM DIOXIDE NANOFIBER CONTAINING ZINC OXIDE NANOPARTICLES USING AN ELECTROSPINNING METHOD AND AN ANTIBACTERICIDAL APPLICATION OF THE SAME UNDER ULTRAVIOLET RAYS AND VISIBLE RAYS OR WITHOUT LIGHT IRRADIATION, CAPABLE OF IMPROVING THE ANTIBACTERICIDAL CAPACITY OF TITANIUM DIOXIDE NANOFIBER CONTAINING ZINC OXIDE NANOPARTICLES

FABRICATION OF TITANIUM DIOXIDE NANOFIBER CONTAINING ZINC OXIDE NANOPARTICLES USING AN ELECTROSPINNING METHOD AND AN ANTIBACTERICIDAL APPLICATION OF THE SAME UNDER ULTRAVIOLET RAYS AND VISIBLE RAYS OR WITHOUT LIGHT IRRADIATION, CAPABLE OF IMPROVING THE ANTIBACTERICIDAL CAPACITY OF TITANIUM DIOXIDE NANOFIBER CONTAINING ZINC OXIDE NANOPARTICLES

机译:使用静电纺丝法制造含有氧化锌纳米粒子的二氧化钛纳米纤维,并在紫外线和可见光下或在无光辐射的情况下,对其进行抗菌和抗菌应用,可改善纳米级的氧化铜

摘要

PURPOSE: Fabrication of titanium dioxide nanofiber containing zinc oxide nanoparticles and an antibactericidal application of the same are provided to easily fabricate titanium dioxide nanofiber containing zinc oxide nanoparticles using a mixed solution of a titanium dioxide precursor, a zinc oxide precursor, and a polymer.;CONSTITUTION: Fabrication of titanium dioxide nanofiber includes the following steps of: preparing the mixed solution of a titanium dioxide precursor, a zinc oxide precursor, polymer, and acetic acid; preparing polymer nanofiber, in which the titanium dioxide precursor and the zinc oxide precursor are mixed, by an electrospinning method; forming titanium dioxide from the titanium dioxide precursor by hydrolysis; and preparing titanium dioxide nanofiber containing zinc oxide nanoparticles by thermally treatment. The sizes of the voltages in the electrospinning method are in a range between 1-60kV. The thermal treatment temperature is in a range between 400-550°C, and the thermal treatment time is in a range between 1 and 4 hours.;COPYRIGHT KIPO 2013
机译:用途:提供包含二氧化钛纳米纤维的二氧化钛纳米纤维的制备及其杀菌应用,以使用二氧化钛前体,氧化锌前体和聚合物的混合溶液容易地制备含有氧化锌纳米颗粒的二氧化钛纳米纤维。组成:二氧化钛纳米纤维的制造包括以下步骤:制备二氧化钛前体,氧化锌前体,聚合物和乙酸的混合溶液;通过静电纺丝法制备混合有二氧化钛前体和氧化锌前体的聚合物纳米纤维。通过水解由二氧化钛前体形成二氧化钛;热处理制备含氧化锌纳米粒子的二氧化钛纳米纤维。电纺丝方法中的电压大小在1-60kV之间的范围内。热处理温度在400-550℃之间,热处理时间在1-4小时之间。; COPYRIGHT KIPO 2013

著录项

  • 公开/公告号KR20130070333A

    专利类型

  • 公开/公告日2013-06-27

    原文格式PDF

  • 申请/专利权人 SNU R&DB FOUNDATION;

    申请/专利号KR20110137601

  • 发明设计人 JANG JYONG SIK;HWANG SUN HYE;SONG HEE;

    申请日2011-12-19

  • 分类号B82B3/00;D01F9/08;B82Y40/00;

  • 国家 KR

  • 入库时间 2022-08-21 16:26:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号