In an industrial purple nano-needle tungsten oxide preparation method, ammonium paratungstate 5(NH4)2O.12WO3.5H2O, tungstic acid mWO3.nH2O (m=1, n=1), or tungsten oxide WOx (2@x@3) is used as a raw material for preparing the purple nano-needle tungsten oxide in an inclined rotating furnace pipe. At an inlet of the furnace pipe, the raw material is pushed from a feed inlet of a feeding device into the heated furnace pipe. The inclined furnace pipe is rotated to gradually move the raw material from a low temperature area to a high temperature area. The raw material at the high temperature area inside the furnace pipe is reduced by H2 to form the nano-needle purple tungsten oxide. The inclined furnace pipe is rotated to move the WO2.72 towards a discharging end, and the purple tungsten oxide WO2.72 is discharged from a discharge outlet of a discharging device and cooled to room temperature by the discharging device.
机译:在工业紫色纳米针状氧化钨的制备方法中,仲钨酸铵5(NH4)2O.12WO3.5H2O,钨酸mWO3.nH2O(m> = 1,n> = 1)或氧化钨WOx(2 @ x @ 3)用作在倾斜的旋转炉管中制备紫色纳米针状氧化钨的原料。在炉管的入口处,将原材料从进料装置的进料口推入加热的炉管中。旋转倾斜的炉管以使原料逐渐从低温区域移动到高温区域。炉管内高温区域的原料被H2还原,形成纳米针状紫色氧化钨。旋转倾斜的炉管以使WO2.72向着排出端移动,紫色氧化钨WO2.72从排出装置的排出口排出,并通过该排出装置冷却至室温。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号