PPROBLEM TO BE SOLVED: To provide a ferritic stainless steel which has all of superior thermal fatigue characteristics, oxidation resistance and high-temperature salt-corrosion resistance though Mo, W and Cu are not added thereinto. PSOLUTION: The ferritic stainless steel has a component composition containing, by mass%, 0.015% or less C, 1.0% or less Si, 0.5% or less Mn, 0.040% or less P, 0.010% or less S, 0.03 to 0.30% Al, 16 to 20% Cr, 0.5% or less Ni, 0.015 to 0.030% N, 0.30 to 0.60% V, 10(C+N) to 0.60% Nb, 0.01% or less Ti, 0.01% or less Zr, 0.01% or less Ta, 0.1% or less Mo, 0.1% or less W while V and N satisfy the relation of (V×N)=0.003 to 0.015, and the balance Fe with unavoidable impurities. PCOPYRIGHT: (C)2010,JPO&INPIT
机译:

要解决的问题:提供一种铁素体不锈钢,尽管不向其中添加Mo,W和Cu,但它们具有所有优异的热疲劳特性,抗氧化性和高温耐盐腐蚀性。

溶液:铁素体系不锈钢的成分组成按质量%计为0.015%以下C,1.0%以下Si,0.5%以下Mn,0.040%以下P,0.010%以下S,0.03。至0.30%Al,16至20%Cr,0.5%以下Ni,0.015至0.030%N,0.30至0.60%V,10(C + N)至0.60%Nb,0.01%以下Ti,0.01%以下Zr,0.01%以下的Ta,0.1%以下的Mo,0.1%以下的W,而V和N满足(V×N)= 0.003〜0.015的关系,余下的Fe具有不可避免的杂质。

版权:(C)2010,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号