A graded porous multi-layered reactive coating method for a shaped charge liner using low temperature spray coating, given in the present invention, includes: a heating and pressurizing step (S120) of heating and pressurizing process gas to make the gas reach a preset temperature and a preset pressure; an acceleration step (S130) of accelerating the gas to supersonic speed by being compressed and expanded while passing through a nozzle (25); a powder supply step (140) of supplying powder for enacting a thermite reaction stored separately from the process gas into the nozzle where the process gas flows to transfer the powder along the nozzle; a powder spray step of spraying the powder which is accelerated by the process gas while moving together with the process gas within the nozzle from the nozzle onto the surface of a basic material (S) which is to be a liner for a shaped charge; and a plastic deformation step of forming a highly-reactive coating layer through plastic deformation on the surface of the basic material by making the powder from the nozzle collide with the basic material. The liner for a shaped charge having a highly-reactive layer manufactured by the method described above has a highly-reactive coating layer (13a) which comprises: a surface coating layer (13aa) which does not have pores from the surface of the liner to a certain depth; and a graded porous coating layer (13ab) of which the pore density decreases as the depth from the surface of the liner grows. [Reference numerals] (AA) Pore density (%); (BB) Depth from the surface(關m)
机译:本发明给出的一种使用低温喷涂的用于成形装药衬里的分级多孔多层反应涂层方法,包括:加热和加压工艺气体以使气体达到预设温度的加热和加压步骤(S120)。和预设压力;加速步骤(S130),其通过在通过喷嘴(25)时被压缩和膨胀而将气体加速到超音速。粉末供给步骤(140),其用于将与处理气体分开存储的用于进行铝热反应的粉末供给到喷嘴中,在喷嘴中,处理气体流动以使粉末沿喷嘴转移。粉末喷涂步骤,其将与工艺气体一起加速的粉末与喷嘴内的工艺气体一起从喷嘴移动到喷嘴上,该基本材料将成为成形装料的衬里;塑性变形步骤是通过使来自喷嘴的粉末与基础材料碰撞而在基础材料的表面上进行塑性变形而形成高反应性的涂层的步骤。通过上述方法制造的具有高反应性层的用于成形装料的衬里具有高反应性涂层(13a),其包括:表面涂层(13aa),该表面涂层从衬里的表面到表面没有孔。一定深度梯度多孔涂层(13ab),其孔隙密度随着从衬里表面的深度的增加而降低。 [参考数字](AA)孔密度(%); (BB)表面深度(关m)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号