The rare earth permanent magnet alloy flexible sintering method and the sintering equipment perform the following processing steps. 1. The fine powder of the rare earth permanent magnet alloy is weighed in a compressor in an inert gas, placed in a mold, made into a semi-finished product by orientation molding, and this semi-finished product is placed in a material container. 2. After the air between the second transport sealed box and the 1 # isolation valve of the glove box is exchanged with an inert gas, the two contacted valves are opened and the bottom roller transport device in the second transport sealed box is When the material placing plate is carried into the 1 # chamber of the glove box and the two isolation valves are closed, the second transfer sealed box is released. 3. The first transfer sealed box is brought into contact with the 3 # isolation valve on the 2 # chamber side, and the flanges of the two contacted isolation valves are hermetically locked. 4). The first conveying hermetic box and the isolation valve of the sintering furnace are brought into contact with each other, and the contacted flange is hermetically locked. 5. When the sintering furnace is evacuated and the degree of vacuum is higher than 50 Pa or a protective gas is introduced, heat insulation is performed with a preset processing curve, and sintering is performed at a maximum temperature of 1200 ° C. The present invention can effectively improve the characteristics of the magnetic material.
机译:稀土永磁合金柔性烧结方法和烧结设备执行以下处理步骤。 1.将稀土永磁体合金的细粉在惰性气体中的压缩机中称重,放入模具中,通过定向成型将其制成半成品,并将该半成品放入物料容器中。 2.用惰性气体交换第二个运输密封箱与手套箱的1#隔离阀之间的空气后,打开两个接触阀,第二个运输密封箱中的下辊运输装置处于将放置板运送到杂物箱的1#腔室中,关闭两个隔离阀,释放第二个转移密封箱。 3.使第一个传输密封盒与2#腔室侧的3#隔离阀接触,并且两个接触的隔离阀的法兰被气密锁定。 4)。使第一输送密封箱和烧结炉的隔离阀彼此接触,并且所接触的凸缘被气密地锁定。 5.当将烧结炉抽空并且真空度高于50Pa或引入保护气体时,以预定的处理曲线进行隔热,并且在最高温度为1200℃下进行烧结。本发明可以有效地改善磁性材料的特性。

著录项

  • 公开/公告号JP2015511271A

    专利类型

  • 公开/公告日2015-04-16

    原文格式PDF

  • 申请/专利号JP20140555066

  • 发明设计人 孫宝玉;陳暁東;

    申请日2013-02-05

  • 分类号B22F3/10;C22C1/04;B22F3;F27D11/02;H01F41/02;H01F1/057;H01F1/08;

  • 国家 JP

  • 入库时间 2022-08-21 15:31:25

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号