Cement solidification formulation and solidification method used for high-concentration boron-containing radioactive waste resin in nuclear power plants

机译:用于核电厂中高浓度含硼放射性废树脂的水泥固化配方和固化方法

摘要

The present invention relates to a cement solidification formulation and a solidification method used for high-concentration boron-containing radioactive waste resin in a nuclear power plant. A solidification formulation comprising cement, lime, water, a solidification aid, and an additive. (1) Weighing the raw material and high-concentration boron-containing radioactive waste resin, first adding lime to the solidification container, (2) adding high-concentration boron-containing radioactive waste resin, (3) Other raw materials while stirring (4) Solidification method including adding cement, adding water according to the dry and wet state of the cement slurry, stirring until uniform, and (5) curing after standing uniformly. The solidification formulation has a high solidification confinement rate, high strength of the solidified body, good water resistance, strong freeze-thaw resistance, and low radioactive leaching rate. The solidification method has low process requirements, is easy to operate, is easy to implement, and can satisfy the demand for solidification on site. [Selection] Figure 1
机译:水泥固化剂和固化方法技术领域本发明涉及用于核电站中的高浓度含硼放射性废树脂的水泥固化剂和固化方法。一种固化配方,包括水泥,石灰,水,固化助剂和添加剂。 (1)称量原料和高浓度含硼放射性废树脂,首先将石灰添加到固化容器中;(2)添加高浓度含硼放射性废树脂;(3)搅拌下的其他原料(4 )固化方法包括添加水泥,根据水泥浆的干湿状态添加水,搅拌至均匀,(5)均匀放置后固化。该固化制剂具有高的固化限制速率,高的固化体强度,良好的耐水性,强的抗冻融性和低的放射性浸出率。该固化方法工艺要求低,易于操作,易于实施,能够满足现场固化的需求。 [选择]图1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号