A rare earth ion doped silicate luminescence glass and preparation method thereof are provided. The luminescence glass is the material with the following formula: aM2O.bM′2O3.cSiO2.dRE2O3, wherein M is at least one of Na, K and Li, M′ is at least one of Y, Gd, La, Sc and Lu, RE is at least one of Ce, Tm, Tb, Ho, Dy, Er, Nd, Sm, Eu and Pr. The preparation method is: grinding the raw material until mixed uniformly, calcining the raw material at 1200-1500° C. for 1-5 h, cooling to room temperature, annealing at 600-1100° C. for 0.5-24 h, cooling to room temperature again, molding then getting the product. The performance of the product is stable. The product is homogenous, and the luminescence performance is good. The light transmittance is high. The process of the preparation method is simple and with low cost.
机译:提供了一种稀土离子掺杂的硅酸盐发光玻璃及其制备方法。发光玻璃是具有下式的材料:aM 2 O.bM′ 2 O 3 .cSiO 2 .dRE 2 O 3 ,其中M为Na,K和Li中的至少一个,M'为Y,Gd,La,Sc和Lu中的至少一个RE是Ce,Tm,Tb,Ho,Dy,Er,Nd,Sm,Eu和Pr中的至少一种。制备方法是:将原料研磨至均匀混合,在1200-1500℃下煅烧1-5小时,冷却至室温,在600-1100℃下退火0.5-24h,冷却再次恢复到室温,成型后得到产品。产品性能稳定。产物均匀,发光性能良好。透光率高。该制备方法的工艺简单,成本低。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号