AGGLOMERATED STONE FOR USING IN SHAFT, COREX OR BLAST FURNACES, METHOD FOR PRODUCING AGGLOMERATED STONES AND USE OF FINE AND SUPERFINE IRON ORE DUST

机译:用于竖炉,高炉或高炉的聚结石材,聚结石材的生产方法以及细铁矿粉和超细铁矿粉的使用

摘要

In order to also be able to economically use iron ore dust which is created by the extraction and preparation of iron ore and has not been usable until now, the invention proposes an agglomerated stone comprising (in wt. %) 6 - 15% of a cement binding agent, up to 20% of a carbon carrier, up to 20% of residual and recyclable substances, optionally up to 10% of a coagulation and solidification accelerator and the remainder consisting of iron ore in a stone format in the form of particles having a particle size of less than 3 mm as well as possessing after three days an initial strength of at least 5 N/mm2 and after 28 days a cold compression strength of at least 20 N/mm2. As a result of the particular hardness St and form stability thereof even at high temperatures T, agglomerated stones according to the invention are especially suitable for use in shaft, corex or blast furnaces. The invention also relates to a method for producing agglomerated stones according to the invention.
机译:为了也能够经济地使用由铁矿石的提取和制备所产生的铁矿石粉尘,并且直到现在才可以使用,本发明提出了一种块状石材,其包含(以重量%计)6-15%的铁矿石。水泥粘结剂,最多20%的碳载体,最多20%的残留和可循环利用的物质,可选地最多10%的凝结和凝固促进剂,其余部分由铁矿石组成,呈颗粒状具有小于3mm的粒度并且在三天后具有至少5N / mm 2的初始强度并且在28天后具有至少20N / mm 2的冷压缩强度。由于特定的硬度St及其即使在高温T下的形状稳定性,根据本发明的结石尤其适用于竖炉,型芯炉或高炉。本发明还涉及一种根据本发明的生产结块石的方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号