PROBLEM TO BE SOLVED: To provide a lean duplex stainless steel laser-weld member in which difference between: property of a weld metal part and of a heat-affected zone; and property of a base metal.SOLUTION: The lean duplex stainless steel laser-weld member with good property of a laser weld part is provided in which a weld metal part is formed by welding a lean duplex stainless steel material having a predetermined chemical composition and area ratio of an austenite phase of 40% to 70% by a laser weld without using a filler metal, and in which the weld metal part has the austenite phase deposited on a grain boundary of a ferrite phase and having an average of width of a cross section of 2.5 μm or more, and the weld member has a calculated value of a deposition initiation temperature of Cr nitride Nof 1250°C or less. N=800 N-3Cr+20Si+10 Ni-4Mn+1140... (1). In the formula (1), Nrepresents nitrogen concentration (mass%) in the weld metal part and each element symbol represents content (mass%) of such element in the steel material.SELECTED DRAWING: None
机译:解决的问题:提供一种精益的双相不锈钢激光焊接构件,该焊接构件之间的区别在于:焊接金属零件的性质和热影响区的性质;解决方案:提供一种具有激光焊接部件的良好性能的贫双相不锈钢激光焊接部件,其中,通过焊接具有预定化学成分的贫双相不锈钢材料形成焊接金属部件,并且在不使用填充金属的情况下,通过激光焊接使奥氏体相的面积比为40%〜70%,并且在焊接金属部中,奥氏体相沉积在铁素体相的晶界上,且平均宽度为截面为2.5μm以上,并且焊接构件具有氮化铬Nof No.1250℃以下的沉积开始温度的计算值。 N = 800N-3Cr + 20Si + 10Ni-4Mn + 1140 ...(1)。式(1)中,N表示焊接金属零件中的氮浓度(质量%),各元素符号表示钢材中该元素的含量(质量%)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号