PROBLEM TO BE SOLVED: To provide a method which can produce rhenium sulfide with little impurity having a shape suitable for improving a volatilization ratio of rhenium in calcination, and can produce high-purity perrhenic acid from this rhenium sulfide by using a dry process.SOLUTION: The method for producing rhenium sulfide comprises: a step of passing an acidic solution containing rhenium through an anion exchange resin to have rhenium adsorbed by the anion exchange resin; a step of passing as an eluent a hydrochloric acid-containing solution containing zinc through the anion exchange resin by which rhenium is adsorbed to elute rhenium therefrom; and a step of subjecting rhenium contained in a liquid after elution to a sulfidation treatment to obtain rhenium sulfide having a zinc concentration of 0.5 mass% or less.
机译:要解决的问题:提供一种方法,该方法可以生产出几乎没有杂质的硫化rh,其形状适合于煅烧中提高improving的挥发率,并且可以通过干法从该硫化rh生产高纯度的高hen酸。 :硫化rh的制备方法包括:使含有containing的酸性溶液通过阴离子交换树脂以使rh被阴离子交换树脂吸附的步骤;使含有锌的含盐酸溶液作为洗脱液的步骤通过吸附exchange的阴离子交换树脂以从中洗脱rh;将洗脱后的液体中含有的ium进行硫化处理,得到锌浓度为0.5质量%以下的硫化rh的工序。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号