LOW EMISSIVITY COATING WITH LOW SOLAR HEAT GAIN COEFFICIENT, ENHANCED CHEMICAL AND MECHANICAL PROPERTIES AND METHOD OF MAKING THE SAME

机译:具有低太阳能热增益系数的低发射率涂层,增强的化学和机械性能以及相同的制造方法

摘要

PROBLEM TO BE SOLVED: To provide a low-emissivity stack having a low solar heat gain coefficient (SHGC), enhanced aesthetics, mechanical and chemical durability, and a tolerance for tempering or heat strengthening, and to provide a method for depositing a coating onto a substrate.SOLUTION: A low-emissivity coating is provided which comprises, in order outward from a substrate: a first dielectric layer; a first nucleation layer; a first Ag layer; a first barrier layer; a second dielectric layer; a second nucleation layer; a second Ag layer; a second barrier layer; a third dielectric layer; and optionally, a topcoat layer. The coating does not contain an independent absorbing layer. In a method for low-emissivity coating, at least one of the first and the second absorbing barrier layers is not fully oxidized, the oxidation state of the absorbing barrier layer that is not fully oxidized is based on sputtering the layer using a ratio of oxygen flow to sputtering power (in kilowatts) that is from 7.5:1 to 8.0:1.
机译:要解决的问题:提供一种具有低太阳热增益系数(SHGC),增强的美观性,机械和化学耐久性以及对回火或热增强的耐受性的低发射率电池组,并提供一种在其上沉积涂层的方法解决方案:提供一种低发射率涂层,该涂层包括从基板向外依次包括:第一介电层;和第一基板。第一成核层;第一Ag层;第一阻挡层;第二介电层;第二成核层;第二Ag层;第二阻挡层;第三介电层;以及任选的面涂层。该涂层不包含独立的吸收层。在用于低发射率涂覆的方法中,第一吸收阻挡层和第二吸收阻挡层中的至少一个没有被完全氧化,未被完全氧化的吸收阻挡层的氧化态基于使用氧的比率溅射该层的方式。流向溅射功率(以千瓦为单位),从7.5:1到8.0:1。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号