首页> 外国专利> Method for producing a metal oxide, zinc oxide solid solution particles, a method of manufacturing a spherical powder, manufacturing method, and cosmetics manufacturing method of coating spherical powder

Method for producing a metal oxide, zinc oxide solid solution particles, a method of manufacturing a spherical powder, manufacturing method, and cosmetics manufacturing method of coating spherical powder

机译:金属氧化物,氧化锌固溶体粒子的制造方法,球状粉体的制造方法,制造方法以及包覆球状粉体的化妆品的制造方法

摘要

PROBLEM TO BE SOLVED: To provide: metal oxide-zinc oxide solid solution particles controllable of a particle size and a form by a simple, inexpensive and environment-friendly method; and coated spherical powder formed by coating, with a hydrophobic compound, the surface of spherical powder obtained by aggregating the metal oxide-zinc oxide solid solution particles, and to provide a cosmetic having an excellent feeling of use by formulating the coated spherical powder.;SOLUTION: This invention relates to: spherical powder which is produced by mixing a water-soluble zinc compound, glycol, an amine compound, and one or two or more kinds of metal salts having a charge of ≤+4, by performing a soft solution reaction at 50°C-100°C, and by accumulating metal oxide-zinc oxide solid solution particles with a primary particle size of 2-200 nm; and which has a spherical form with the size of 10-5,000 nm; or to coated spherical powder which is formed by using spherical powder obtained by firing the spherical powder at 300°C-1,500°C, and by coating the surface of the spherical powder with one or two or more kinds of compounds selected from polysiloxane, an alkyl alkoxysilane compound, an alkyl titanate compound and a fluorine compound. A cosmetic formed by formulating the coated spherical powder is also provided.;COPYRIGHT: (C)2013,JPO&INPIT
机译:解决的问题:提供:通过简单,廉价且环境友好的方法可控制粒度和形态的金属氧化物-氧化锌固溶体颗粒;通过将疏水性化合物的金属氧化物-氧化锌固溶体粒子凝集而得到的球形粉末的表面被疏水性化合物包覆而形成的包覆球形粉末,通过配制该包覆球形粉末而提供使用感优异的化妆品。解决方案:本发明涉及:球形粉末,其是通过将水溶性锌化合物,二醇,胺化合物以及一种或两种或更多种电荷≤+ 4的金属盐通过软溶液混合而制得的在50℃至100℃下反应,并积聚一次粒径为2-200nm的金属氧化物-氧化锌固溶体颗粒。球形,尺寸为10-5,000 nm;或涂覆的球形粉末,其是通过使用在300℃至1,500℃下煅烧球形粉末并通过用选自聚硅氧烷中的一种或两种以上的化合物涂覆球形粉末的表面而形成的球形粉末形成的。烷基烷氧基硅烷化合物,钛酸烷基酯化合物和氟化合物。还提供了一种通过配制包覆的球形粉末而形成的化妆品。;版权所有:(C)2013,日本特许厅&INPIT

著录项

  • 公开/公告号JP5872825B2

    专利类型

  • 公开/公告日2016-03-01

    原文格式PDF

  • 申请/专利权人 大東化成工業株式会社;

    申请/专利号JP20110198551

  • 发明设计人 後藤 武弘;田中 巧;

    申请日2011-09-12

  • 分类号A61K8/27;A61Q17/04;A61Q1/02;A61Q1/10;A61Q1/04;C01G9/00;

  • 国家 JP

  • 入库时间 2022-08-21 14:40:42

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号