首页> 外国专利> Method for Manufacturing a Kraft Fiber comprising oxygen and deslignificar Digest with a Softwood Pulp Kappa number to between 6 and 14, bleaching the Pulp bleaching process using a multiple stages and meant oxidising it during at least one stage of the bleaching process With multiple stages, and a Peroxide Catalyst under acid conditions (Divisional no. 3005 - 11)

Method for Manufacturing a Kraft Fiber comprising oxygen and deslignificar Digest with a Softwood Pulp Kappa number to between 6 and 14, bleaching the Pulp bleaching process using a multiple stages and meant oxidising it during at least one stage of the bleaching process With multiple stages, and a Peroxide Catalyst under acid conditions (Divisional no. 3005 - 11)

机译:制造包含氧气和软木纸浆卡伯值在6至14之间的令人满意的消化物的牛皮纸纤维的方法,使用多阶段漂白纸浆漂白过程,并且意指在漂白过程的至少一个阶段中将其氧化,并进行多步漂白;以及酸性条件下的过氧化物催化剂(部门编号3005-11)

摘要

a. The method for manufacturing Kraft fiber includes: adsorbing cellulose fiber to kappa number of 6-14 and separating it with oxygen; bleaching cellulose with a polygonal bleaching process; The Kraft fiber was oxidized by peroxide and catalyst at least for one stage. In this stage, the mixed bleaching process includes at least one bleaching stage, and then the oxidation stage.
机译:一种。制造牛皮纸纤维的方法包括:将纤维素纤维吸附至卡伯值为6-14,并用氧气将其分离。用多边形漂白工艺漂白纤维素;将牛皮纸纤维至少用一级过氧化物和催化剂氧化。在这一阶段,混合漂白过程包括至少一个漂白阶段,然后是氧化阶段。