A visible-light-responsive photocatalyst powder includes a tungsten oxide powder. When the tungsten oxide powder is measured by X-ray diffractometry, (1) among intensity ratios of a peak A (2θ=22.8 to 23.4°), a peak B (2θ=23.4 to 23.8°), a peak C (2θ=24.0 to 24.25°), and a peak D (2θ=24.25 to 24.5°), an A/D ratio and a B/D ratio each fall within a range of 0.5 to 2.0, and a C/D ratio falls within a range of 0.04 to 2.5, (2) an intensity ratio (E/F) of a peak E (2θ=33.85 to 34.05°) to a peak F (2θ=34.05 to 34.25°) falls within a range of 0.1 to 2.0, and (3) an intensity ratio (G/H) of a peak G (2θ=49.1 to 49.7°) to a peak H (2θ=49.7 to 50.3°) falls within a range of 0.04 to 2.0, and the tungsten oxide powder has a BET specific surface area in a range of 1.5 to 820 m2/g.
机译:可见光响应型光催化剂粉末包括氧化钨粉末。当通过X射线衍射法测量氧化钨粉末时,(1)在峰A(2θ= 22.8至23.4°),峰B(2θ= 23.4至23.8°),峰C(2θ= 24.0〜24.25°),峰D(2θ= 24.25〜24.5°),A / D比和B / D比分别在0.5〜2.0的范围内,C / D比在该范围内。在0.04至2.5的范围内,(2)峰E(2θ= 33.85至34.05°)与峰F(2θ= 34.05至34.25°)的强度比(E / F)在0.1至2.0的范围内,并且(3)峰G(2θ= 49.1至49.7°)与峰H(2θ= 49.7至50.3°)的强度比(G / H)在0.04至2.0的范围内,氧化钨粉末具有BET比表面积为1.5至820 m 2 / g。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号