首页> 外国专利> Polyurethane composite material, preferably in the form of shaped blocks for applications in hydroengineering for construction of flood banks and/or reinforcement of berths and method for producing it

Polyurethane composite material, preferably in the form of shaped blocks for applications in hydroengineering for construction of flood banks and/or reinforcement of berths and method for producing it

机译:聚氨酯复合材料,优选为成型块的形式,用于水力工程中以建造防洪堤和/或泊位的加固及其生产方法

摘要

the object of the application is composite, containing phosphogypsum; fly ash, boiler dust and slag, which is characterized by the fact that additionally contains from 1% to 50% parts by weight of rubber and 1% - 30% by weight of polyurethane, and water in quantities dopeu0142niaju0105cej to 100% by weight.the subject application is also a way of composition, which is that preparing a mixture consisting of from 1% to 40% by weight fosfogipsu, from 1% to 40% by weight of volatile, 1% to 40% by weight of boiler dust and slag, and from 1% to 50% by weight of gr anulatu rubber, and then to the weight of the mixed favourably at 30 - 60 rpm,the following dwusku0142adnikowu0105 mass of polyurethane polyols and isocyanates in which mixture mixture ratio 2: 1, the whole is mixed in a gas mixing piece and wtu0142aczana to appropriate forms of steel to perform appropriate of composite.
机译:本申请的目的是包含磷石膏的复合材料。飞灰,锅炉粉尘和炉渣,其特征在于还包含1%至50%重量份的橡胶和1%-30%重量份的聚氨酯,以及水,其用量为100至100本申请也是一种组合物的方法,该方法是制备一种混合物,该混合物由1-40重量%的fosfogipsu,1-40重量%的挥发性,1-40重量%的组成。锅炉粉尘和炉渣,然后从1%到50%的gr ulatutu橡胶,然后以30-60 rpm的转速良好混合,以下聚氨酯多元醇和异氰酸酯的质量为:混合比混合比为2:1,将整个混合物在混合气中混合并混合成适当形式的钢,以进行适当的复合。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号