INK COMPOSITION FOR HIGH-SPEED SCREEN PRINTING, PRINTED MATTER PRODUCED BY THE HIGH SPEED SCREEN PRINTING OF THE INK COMPOSITION, AND METHOD FOR PRODUCING THE PRINTED MATTER

机译:用于高速丝网印刷的油墨组合物,通过该油墨组合物的高速丝网印刷产生的印刷物以及用于生产印刷物的方法

摘要

Ink composition high-speed screen printing, printed article obtained by high-speed, producing width of no more than 10 æm, containing a solvent with a boiling point of not less than 170øC at not less than 70 wt pcnt of the total solvent, and a prepolymer or polymer with a weight-average molecular weight of not less than 2000 at not less than 7 wt pcnt of to the total ink composition, and having a viscosity of not less than 6 Pas and less than 30 Pas as measured with a BH-type rotating viscosimeter at 25øC, and a thixotropic index of 2.0 to 8.0, the measured flow radius value of 14.0 to 24.0 mm after 1 minute from the start according to JIS K5701-1:2000 satisfying "F60" - "F45" = 0. 8 mm, where "F60" and "F45" are severally flow radius value after 1 minute 45 seconds from the start.
机译:油墨组合物高速丝网印刷,通过高速获得的印刷品,其宽度不大于10æm,且在总溶剂中的沸点不小于70 wt%,且其沸点不小于170°C,并且预聚物或重均分子量不小于2000且不小于油墨组合物总量的7 wt%的预聚物或聚合物,用BH测得的粘度不小于6 Pas并且小于30 Pas型旋转粘度计,温度为25°C,触变指数为2.0至8.0,从JIS K5701-1:2000开始算起1分钟后,测得的流动半径值为14.0至24.0 mm,满足“ F60”-“ F45” = 0 8毫米,其中“ F60”和“ F45”分别是从开始起1分45秒后的流动半径值。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号