Provided is a method for producing nano silicon dioxide and nano calcium carbonate by using rice hull ash and flue gas of a biomass power plant. The method comprises: adding the rice hull ash into a sodium hydroxide solution, fully reacting at the temperature of 95-100 °C for 3-4 hours, and performing filtration; adding water into a filtrate to dilute the filtrate, controlling sodium silicate in a system to be 8-15 wt% in silicon dioxide, heating to 60-80 °C, adding a dispersing agent, continuously feeding the flue gas of the biomass power plant under a normal pressure condition, stirring to react for 2-4 hours to obtain the nano silicon dioxide; mixing the filtrate and a washing liquid, adding a calcium hydroxide solution at the temperature of 50-70 °C, and stirring to react for 0.5-2 hours to obtain the nano calcium carbonate. The particle sizes of the silicon dioxide product and the calcium carbonate product which are obtained by the method are extremely small and can both reach the nano level.
机译:提供了一种利用稻壳灰和生物质能发电厂的烟气生产纳米二氧化硅和纳米碳酸钙的方法。该方法包括:将稻壳灰加入氢氧化钠溶液中,在95-100℃的温度下充分反应3-4小时,然后进行过滤;向滤液中加水以稀释滤液,控制系统中的硅酸钠含量为二氧化硅的8-15 wt%,加热至60-80°C,添加分散剂,连续给生物质发电厂的烟气供料在常压条件下,搅拌反应2-4小时,得到纳米二氧化硅。将滤液和洗涤液混合,在50-70℃的温度下加入氢氧化钙溶液,搅拌反应0.5-2小时,得到纳米碳酸钙。通过该方法获得的二氧化硅产物和碳酸钙产物的粒度非常小,并且都可以达到纳米级。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号