清浄度鋼の鋳造方法

机译:如何铸造清洁度钢

摘要

PROBLEM TO BE SOLVED: To provide a method for casting cleanliness steel excellent in fatigue resistance.;SOLUTION: A method for casting cleanliness steel comprises adding a coating material containing at least CaO, SiO2 and Al2O3 into a tundish 2 of a continuous casting facility 1 upon casting cleanliness steel in the continuous casting facility 1. In the method for casting cleanliness steel, a coating material whose basicity is adjusted is added such that the basicity of a slag in the tundish 2 at an end of casting is of a value at which balance is achieved in a formula (1) or greater in accordance with an Al concentration of molten steel to be cast. 4Al+3SiO2=3Si+2Al2O3...(1);SELECTED DRAWING: Figure 1;COPYRIGHT: (C)2019,JPO&INPIT
机译:解决的问题:提供一种耐疲劳性优良的洁净钢的铸造方法;解决方案:洁净钢的铸造方法包括添加至少包含CaO,SiO 2 和Al 2 O 3 在连续铸造设备1中浇铸洁净钢时,在连续铸造设备1的中间包2中浇铸。添加调节量,使得在浇铸结束时中间包2中的炉渣的碱度具有根据待铸造的钢水的Al浓度在式(1)以上达到平衡的值。 4Al + 3SiO 2 = 3Si + 2Al 2 O 3 ...(1);选定的图纸:图1;版权:(C) 2019年,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号