To solve a problem of causing a surface defect called orange peel such as a rough surface, a pore or distortion in a shaped article by shaping using a recycled resin powder for stereoscopic shaping, or decreasing tensile strength of the shaped article.SOLUTION: There is provided resin powder for stereoscopic shaping, comprising: a melting point of 100°C or higher by measuring in accordance with ISO 3146; and a ratio of greater than 0.80 and less than 1.20 in dividing of a melt mass flow rate after keeping a temperature by a melt mass flow rate before keeping the temperature, when the melt mass flow rates before and after keeping at a temperature of 15°C lower than a melting point at a pressure of 0.1 kPa for 4 hours are measured under conditions of a load of 2.16 kg and a temperature of 15°C higher than the melting point in accordance with JIS K7210.SELECTED DRAWING: None
机译:为了解决这样的问题,即通过使用再生树脂粉末进行立体成型来成型或降低成型品的拉伸强度,从而在成型品中引起诸如桔皮之类的表面缺陷(如粗糙的表面),孔洞或变形,或降低成型品的拉伸强度。提供的用于立体成形的树脂粉末,其包括:通过根据ISO 3146的测量,熔点为100℃或更高;以及保持温度前后的熔体质量流量为15°时,将保持温度后的熔体质量流量除以保持温度前的熔体质量流量的比值大于0.80且小于1.20。根据JIS K7210,在2.16 kg的载荷和高于熔点15°C的温度下,以0.1 kPa的压力在4小时内低于熔点的C.

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号