High Temperature Chloride Corrosion Resistant NiCrTiAlSi/La2O3 Coating at Flue Gas Side of Waste Incineration Power Generating Boiler and Preparation Method Thereof

机译:垃圾焚烧发电锅炉烟气侧的耐高温氯化物腐蚀NiCrTiAlSi / La2O3涂层及其制备方法

摘要

Provided are a high temperature and chloride corrosion resistant NiCrTiAlSi/La2O3 coating at a flue gas side of a waste incineration power generating boiler and a preparation method thereof. The method comprises the following steps: (1) preparing a composite powder; (2) uniformly grinding the composite powder to obtain a spherical composite powder, then drying the spherical composite powder; (3) cleaning and roughening a surface of a substrate; (4) using a thermal spraying technique to spray a primer layer on a heating surface; (5) using a thermal spraying technique to spray the spherical composite powder onto the primer layer; and (6) cooling. The coating obtained by the method comprises a composite coating spray-coated on a surface of the primer layer. A rare element in the form of La2O3 is added to the coating to purify a grain boundary of the coating. The method strengthens the grain boundary and promotes the formation of an oxide film to alter the morphology of the coating, refine a crystal grain, and improve a high temperature and corrosion resistance and oxidation resistance of the coating.
机译:提供了一种在垃圾焚烧发电锅炉烟气侧的耐高温,耐氯化物腐蚀的NiCrTiAlSi / La2O3涂层及其制备方法。该方法包括以下步骤:(1)制备复合粉末; (2)将复合粉均匀研磨得到球形复合粉,然后干燥球形复合粉; (3)对基板的表面进行清洁和粗糙化处理; (4)采用热喷涂技术在加热面上喷涂底漆层; (5)采用热喷涂技术将球形复合粉末喷涂到底漆层上; (6)冷却。通过该方法获得的涂层包括喷涂在底漆层的表面上的复合涂层。将La 2 O 3 形式的稀有元素添加到涂层中,以净化涂层的晶界。该方法增强了晶界并促进了氧化膜的形成,从而改变了涂层的形态,细化了晶粒,并改善了涂层的高温,耐腐蚀性和抗氧化性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号