首页> 外国专利> Semi-flexible pavement cement milk and its manufacturing method and semi-flexible pavement construction method

Semi-flexible pavement cement milk and its manufacturing method and semi-flexible pavement construction method

机译:半柔性路面水泥乳及其制造方法和半柔性路面施工方法

摘要

PROBLEM TO BE SOLVED: To provide a cement milk having low viscosity, which easily penetrates into an open-graded asphalt mixture being a parent body for semiflexible paving material, and having a longer setting start time, while using salt water containing chloride ions, such as sea water used as kneading water.SOLUTION: There is provided a cement milk comprising: cement; a mortar composition including a fast curing admixture and fine aggregate; and salt water of an amount within a range of 20 pts.mass or more and 50 pts.mass or less with respect to 100 pts.mass of the mortar composition. The cement milk also comprises: chloride ions in a range of 1 pts.mass or more and 4 pts.mass or less in the salt water; and a setting modifier of an amount within a range of 0.1 pts.mass or more and 0.7 pts.mass or less with respect to 100 pts.mass of the mortar composition.SELECTED DRAWING: None
机译:解决的问题:提供低粘度的水泥乳,当使用含氯离子的盐水时,该乳容易渗入作为半柔性铺路材料的母体的开放级沥青混合物中,并且凝结开始时间更长。解决方案:提供了一种水泥乳,其包含:水泥;和作为混合物的水泥乳。砂浆组合物,其包含快速固化的混合物和细骨料;以及相对于砂浆组合物的100点质量在20点质量以上且50点质量以下范围内的盐水。所述水泥乳还包含:盐水中的氯离子在1点质量或更高至4点质量或更低的范围内;相对于砂浆组合物的100 pts质量的量在0.1 pts.mass或0.7 pts.mass范围内的量和固化调节剂。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号