Disclosed is a method for preparing a high-performance iron oxide red/clay mineral hybrid pigment by mechanochemistry, the method comprising mixing a clay mineral, a soluble iron source and an alkali source in a mill for grinding so as to obtain a precursor, wherein the ratio of balls to materials is controlled at 20-50, the grinding speed is 300-1200 rpm, and the grinding time is 30-360 min; and then calcining the precursor at 500ºC-900ºC for 30-120 min to obtain the high-performance iron oxide red/clay mineral hybrid pigment. The iron oxide red/clay mineral hybrid pigment has a bright and beautiful color, excellent high-temperature and acid resistance, and can satisfy requirements for high-performance iron oxide red pigments in the fields of paints, inks, ceramics, anti-corrosive coatings, etc. Furthermore, the preparation method of the present invention does not produce the three wastes, and is a simple process that is environmentally friendly and suitable for industrialized production, thus it is expected to replace existing production processes of iron oxide red pigments.
机译:公开了一种通过机械化学制备高性能氧化铁红/粘土矿物杂化颜料的方法,该方法包括在研磨机中混合粘土矿物,可溶性铁源和碱源以研磨以获得前体,其中球与物料的比例控制在20-50,研磨速度为300-1200 rpm,研磨时间为30-360 min。然后在500ºC-900ºC下煅烧前驱体30-120分钟,以获得高性能的氧化铁红/粘土矿物杂化颜料。氧化铁红/粘土矿物杂化颜料色泽鲜艳美丽,具有优异的耐高温和耐酸性,可满足油漆,油墨,陶瓷,防腐涂料领域对高性能氧化铁红颜料的要求此外,本发明的制备方法不产生这三种废物,并且是一种环境友好且适合工业化生产的简单方法,因此有望替代现有的氧化铁红颜料的生产方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号