A high-entropy alloy boride ceramic and a preparation method therefor. The molecular formula of the high-entropy alloy boride ceramic is Aly(FeNiCoCr)1-x-yBx, wherein 0≤x≤1 and 0≤y≤1.The high-entropy alloy boride is prepared by the following steps: carrying out ball milling on Al, Fe, Ni, Co, Cr, and B to prepare Aly(FeNiCoCr)1-x-yBx powder; then carrying out spark plasma sintering at a heating rate of 50-200 °C/min, a temperature of 800-1500 °C, and a constant pressure of 10-50 Mpa; carrying out furnace cooling. The Aly(FeNiCoCr)1-x-yBx high-entropy alloy boride powder prepared by the method is approximately spherical and is small in particle size, the ceramic main phase is an FCC solid solution in which Fe and Cr metal borides are dispersed, and high density, high hardness and wear resistance are achieved.
机译:高熵合金硼化物陶瓷及其制备方法。高熵合金硼化物陶瓷的分子式为Aly(FeNiCoCr)1-x-yBx,其中0≤x≤1和0≤y≤1。通过以下步骤制备高熵合金硼化物:在Al,Fe,Ni,Co,Cr和B上进行球磨以制备Aly(FeNiCoCr)1-x-yBx粉末;然后以50-200℃/ min的升温速率,800-1500℃的温度和10-50MPa的恒压进行火花等离子体烧结;进行炉冷却。通过该方法制备的Aly(FeNiCoCr)1-x-yBx高熵合金硼化物粉末近似球形,粒径小,陶瓷主相为FCC固溶体,其中分散有Fe和Cr金属硼化物,并且实现了高密度,高硬度和耐磨性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号