(Problem) An object of the present invention is to provide a dry-type hollow fiber membrane module having excellent blood compatibility and less eluate, and a method of manufacturing a hollow fiber membrane and a hollow fiber membrane module embedded in the module. (Solution means) A hollow fiber membrane module comprising a hollow fiber membrane containing a hydrophobic polymer and a hydrophilic group-containing polymer and satisfying the following items. (a) the water content of the hollow fiber membrane is 10% by weight or less (b) the hydrophobic polymer does not contain nitrogen, the hydrophilic group-containing polymer contains nitrogen, and the nitrogen content of the hollow fiber membrane is 0.05% by weight or more 2.0 × 10 used for titration for the eluate of 0.4% or less (c) the film said hydrophilic group content of containing polymer with less than 45 wt% to 20 wt.% (d) priming final latex 10mL of the inner surface - Consumption of 3 mol/L potassium permanganate aqueous solution is 0.2mL or less per 1㎡ of membrane area
机译:(问题)本发明的目的是提供血液相容性优异且洗出液少的干式中空纤维膜组件,中空纤维膜的制造方法以及埋入该组件的中空纤维膜组件。 (解决方法)一种中空纤维膜组件,其包括含有疏水性聚合物和含亲水性基团的聚合物且满足以下条件的中空纤维膜。 (a)中空纤维膜的水含量为10重量%或更低(b)疏水聚合物不包含氮,含亲水基的聚合物包含氮,并且中空纤维膜的氮含量为0.05%按重量计大于等于2.0×10的滴定液用于0.4%或以下的洗脱液(c)膜中所含的亲水基团含量小于45 wt%至20 wt。%的聚合物(d)涂底漆10mL内表面- 3 mol / L高锰酸钾水溶液的消耗量为每1平方米膜面积0.2mL以下

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号