ZnO nanowires, nanorods and microrods have been prepared by an organic-free hydrothermal process using ZnSO4 and NaOH/NH4OH solutions. The powder X-ray diffraction (PXRD) patterns reveal that the ZnO nano/microrods are of hexagonal wurtzite structure. The Fourier transform infrared (FT-IR) spectrum of ZnO powder shows only one significant spectroscopic band at around 417 cm-1 associated with the characteristic vibrational mode of Zn-O bonding. The thickness 75-300 nm for ZnO nanorods and 0.2-1.8 μm for microrods are identified from SEM/TEM images. UV-visible absorption spectra of ZnO nano/microrods show the blue shift. The UV band and green emission observed in photoluminescence (PL) spectra are due to free exciton emission and singly ionized oxygen vacancy in ZnO. Finally, the mechanism for organic-free hydrothermal synthesis of the ZnO nano/microrods is discussed. © 2010 Elsevier Ltd. All rights reserved.
机译:ZnO纳米线,纳米棒和微棒已经通过使用ZnSO4和NaOH / NH4OH溶液的无有机水热工艺制备。粉末X射线衍射(PXRD)图谱表明,ZnO纳米/微棒具有六方纤锌矿结构。 ZnO粉末的傅立叶变换红外(FT-IR)光谱在417 cm-1处仅显示出一个与Zn-O键的特征振动模式相关的重要光谱带。 ZnO纳米棒的厚度为75-300 nm,微棒的厚度为0.2-1.8 µm是从SEM / TEM图像中确定的。 ZnO纳米/微棒的紫外可见吸收光谱显示出蓝移。在光致发光(PL)光谱中观察到的UV带和绿色发射是由于ZnO中的自由激子发射和单离子氧空位所致。最后,讨论了无有机物水热合成ZnO纳米/微棒的机理。 ©2010 Elsevier Ltd.保留所有权利。