Method for Direct Determination of Glassy Phase Dissolution in Hydrating Fly Ash-Cement System Using X-ray Diffraction

机译:X射线衍射直接测定水合粉煤灰水泥系统中玻璃相溶解度的方法

摘要

A method for quantitative X-ray diffraction analysis is developed for direct determination of the glassy phase content of fly ash in a hydrating binary blend of cement and low-calcium, siliceous fly ash. The intensity contributions of the unhydrated glassy phase of fly ash and the amorphous reaction products to the intensity pattern of the total amorphous phase in the hydrating binary blend are obtained by decomposition of the total intensity signature as a sum of component pseudo Voigt (PV) peaks. An experimental program involving binary blends with three different low calcium siliceous fly ashes and two different curing temperatures is reported. The centers of the component PV peaks of the fly ash glassy phase fitted to the overall intensity pattern are found to be invariant. The glassy phase content of hydrating binary blends determined from the XRD method were found to agree well with the values obtained from a selective dissolution method.
机译:开发了一种定量X射线衍射分析的方法,用于直接测定水泥与低钙硅质粉煤灰的水合二元混合物中粉煤灰的玻璃相含量。粉煤灰的未水合玻璃态相和无定形反应产物对水合二元混合物中总无定形相的强度分布的强度贡献是通过分解总强度特征作为伪拟Voigt(PV)峰的总和而获得的。报告了一个实验程序,该程序涉及具有三种不同的低钙硅粉煤灰和两种不同的固化温度的二元共混物。发现与总强度图拟合的粉煤灰玻璃状相的组分PV峰的中心是不变的。发现通过XRD方法测定的水合二元混合物的玻璃相含量与通过选择性溶解方法获得的值非常吻合。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号