【2h】

Effect of blending time and crumb rubber content on properties of crumb rubber modified asphalt binder

机译:混合时间和碎胶含量对碎胶改性沥青粘合剂性能的影响

摘要

The increasing use of crumb rubber modifier in flexible pavements justifies the necessity for a better understanding of its physical and rheological properties as well as its elasticity behaviour. Basically the performance and properties of rubberised asphalt binder are influenced by the blending conditions and crumb rubber content. In this study, the laboratory investigation was conducted on crumb rubber modified asphalt binder properties as a function of two blending times (30 minutes and 60 minutes) and five crumb rubber contents (4, 8, 12, 16 and 20 by weight of asphalt binder) at mixing temperature of 180°C. Statistical analysis using two-way ANOVA was conducted on the results to evaluate the significance of rubber contents and blending times. The rubberised asphalt binder was evaluated in terms of binder elasticity and rutting resistance at high temperature. The results indicate that the crumb rubber content had a significant effect on G*/ sin (δ) at 76°C. The higher crumb rubber content appears to dramatically increase the elastic recovery and ductility. Statistical analysis showed significant effect of crumb rubber content in influencing the ductility, elastic recovery and G*/ sin (δ) values. Whereas the blending time do not appears to significantly affect the ductility, elastic recovery and rutting factor (G*/ sin (δ)) of the CRM asphalt binder. The asphalt binder with higher crumb rubber content and longer blending time of 60 minutes exhibited a higher value of elastic recovery. This indicates that crumb rubber modified asphalt binder has better resistance to rutting as compared to conventional asphalt binder.
机译:在柔性路面中越来越多地使用抗碎橡胶改性剂,这证明有必要更好地了解其物理和流变性能以及其弹性性能。基本上,橡胶沥青混合料的性能和性能受混合条件和胶粒含量的影响。在这项研究中,实验室研究了碎橡胶改性沥青粘合剂的性能,该性能是两个混合时间(30分钟和60分钟)和五个碎橡胶含量(分别为沥青粘合剂重量的4、8、12、16和20)的函数)在180°C的混合温度下。使用双向方差分析对结果进行统计分析,以评估橡胶含量和共混时间的重要性。根据高温下的粘合剂弹性和耐车辙性评价了橡胶状沥青粘合剂。结果表明,面包屑的橡胶含量对76°C时的G * / sin(α)有显着影响。较高的碎屑橡胶含量似乎显着增加了弹性回复性和延展性。统计分析表明,碎胶含量在影响延展性,弹性恢复和G * / sin(β)值方面具有显著作用。而共混时间似乎并不显着影响CRM沥青粘合剂的延展性,弹性恢复和车辙系数(G * / sin(η))。具有更高的碎橡胶含量和更长的60分钟混合时间的沥青粘合剂表现出更高的弹性回复值。这表明与常规沥青粘合剂相比,碎橡胶改性沥青粘合剂具有更好的耐车辙性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号