The present study evaluated the influence of different composite bases and surface treatments on marginal and internal adaptation of class II indirect composite restorations, after simulated occlusal loading. Thirty-two class II inlay cavities were prepared on human third molars, with margins located in cementum. A 1-mm composite base extending up to the cervical margins was applied on all dentin surfaces in the experimental groups; impressions were made and composite inlays fabricated. The following experimental conditions were tested: no liner (control group), flowable composite treated with soft air abrasion (experiment 1), flowable composite sandblasted (experiment 2) and restorative composite sandblasted (experiment 3). All specimens were submitted to 1,000,000 cycles with a 100-N eccentric load. Tooth-restoration margins were analysed semi-quantitatively by scanning electron microscopy before and after loading; internal adaptation was also evaluated after test completion. The percentage of perfect adaptation in enamel was 79.5% to 92.7% before loading and 73.3% to 81.9% after loading. Perfect adaptation to dentin was reduced before loading (54.8% to 77.6%) and after loading (41.9% to 63%), but no difference was found among groups for pre- and post-loading conditions. No debonding occurred between the base and composite luting. A significant, negative influence of cyclic loading was observed. The results of the present study support the use of flowable or restorative composites as base/liner underneath large class II restorations. Soft air abrasion represents a potential alternative to airborne particle abrasion for treating cavities before cementation. The application of a composite base underneath indirect composite restorations represents a feasible non-invasive alternative to surgical crown lengthening to relocate cavity margins from an intra-crevicular to supra-gingival position.
机译:本研究评估了模拟咬合载荷后不同复合碱基和表面处理对II类间接复合修复的边缘和内部调整的影响。在人的第三磨牙上制备三十二级镶嵌空腔,位于豆类中的边缘。在实验组中的所有牙本质表面上施加1mm延伸到宫颈边缘的复合底座;制造印象,制作复合镶嵌物。测试以下实验条件:无衬里(对照组),用软空气磨损(实验1)处理的可流动复合材料,可流动复合砂粘剂(实验2)和修复复合砂刺(实验3)。所有标本均用100-N偏心载荷提交至1,000,000个循环。在装载之前和之后通过扫描电子显微镜通过扫描电子显微镜分析牙齿恢复边缘;在测试完成后也评估内部适应。在装载之前,搪瓷完美适应的百分比为79.5%至92.7%,装载后73.3%至81.9%。在装载前(54.8%至77.6%)和装载后的完美适应(54.8%至77.6%)(41.9%至63%),但在预装载条件下,群体中没有发现差异。底座和复合材料之间没有发生借方。观察到循环载荷的显着负面影响。本研究的结果支持使用可流动或修复的复合材料作为底座/衬里下方的II类修复后。软空气磨损代表潜在的替代空气中颗粒磨损以在胶粘剂之前处理空腔。间接复合修复物下方的复合基座的应用代表了一种可行的非侵入性替代物,用于从克里克里克牙龈上迁移腔边缘。