INSERTION OF GALLIUM OXIDE INTO alpha-TITANIUM PHOSPHATE USING A SURFACTANT EXPANDED PHASE AS PRECURSOR

机译:以表面活性剂扩展相为前驱体将氧化镓插入α-磷酸钛中

获取原文
获取原文并翻译 | 示例
           

摘要

Intercalated gallium oxide in alpha-titanium phosphate materials can be synthesized using a swelled phase such as cetyltrimethyl ammonium titanium phosphate as precursor. This is prepared in a single step by hydrolysis of titanium iso-propoxide with phosphoric acid via a supramolecular long-range ordered organic species acting as a template, which by cationic exchange with gallium oligomers and ulterior calcination at 823 K gives rise to mesoporous solids. These materials exhibit high specific surface areas close to 150 m2 g-1, high acidity predominantly of the Lewis type, which are active as catalysts in the conversion of the 2-propanol dehydration reaction at 493 K with conversions ranging between 50 and 83%, and total selectivities for propene. 18 refs.
机译:可以使用诸如十六烷基三甲基铵钛磷酸盐的溶胀相作为前体来合成α-磷酸钛材料中的嵌入氧化镓。它通过一步法通过将超分子远程有序有机物质用作模板,通过磷酸将异丙氧基钛水解,通过与镓低聚物的阳离子交换和在823 K下的进一步煅烧生成介孔固体,从而一步一步制备。这些材料具有接近150 m2 g-1的高比表面积,主要是路易斯型酸度高,在493 K时2-丙醇脱水反应的转化率介于50%到83%之间时,具有催化活性。丙烯的总选择性。 18个参考

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号